Midwest metal fastener manufacturer had a serious problem with the bushings in its new high-tech electrostatic painting line. The components were having trouble performing under three extremely difficult conditions: carrying current, surviving caustic solutions and enduring high temperatures.
The application in question
involved placing batches of small
metal parts to be painted into stainless
steel baskets, then cycling them
through a series of operations during
the painting process. The baskets were
suspended from an overhead conveyor
by supporting rods connected to stub
axles protruding from the sides of
each basket. Metal parts were first
dipped into a caustic cleaning and
de-greasing solvent, treated with a
primer, then immersed into an Ecoat
paint tank. Painted parts were
then cured as they traveled through a
350 F oven.
Because these fully-loaded baskets weighing over 100 lbs. were required to tumble during part of the operation, each would be driven by a sprocket and heavy-duty chain to achieve the necessary rotation (see diagram). Since paint would be applied electrostatically, the baskets were charged with 360 volts DC of electricity supplied from an overhead power source and transmitted to the baskets and parts via the chain/ sprocket/axle assembly.
An arcing problem
Soon after starting up the new
painting line, the plant’s production
manager discovered a problem. The
combination of high voltage coupled
with a weak point of contact along the
transmission circuit—specifically the
axle to basket housing—was causing
arcing and sparking problems. The
situation was so extreme that it was
actually pitting and melting metal
components. Entire sections of chain,
for example, were being “eaten away”
by the electrical charges!
To the rescue
John Graff, engineering representative
with Graphite Metallizing Corporation,
was invited in to review the
application. Established in 1913, this
company produces GRAPHALLOY,
a graphite-metal alloy used in the
manufacture of bushings, bearings
and discrete components for
machinery and process systems.
Graff knew that the high temperature and corrosive environment were key problems, but that any solution would have to eliminate the arcing on the chain. In light of GRAPHALLOY’s electrical-conducting capabilities, he recommended an iron GRAPHALLOY bearing in a cast iron flanged housing, the combination of which would provide an effective path for the current flow.
The flanged units solved the “triple threat” problem. The path of electrical transmission was controlled and the arcing problem was eliminated. The bushings also survive caustic solvents and the application’s high heat environment. Furthermore, they’re maintenance-free. That’s because the chemical and mechanical properties of these components are so unique that they never need lubrication and perform exceptionally well in applications where other bearings would easily fail.
Graphite Metallizing Corporation
Yonkers, NY